Oxidation Failure Behavior of Cr-Coated Zirconium Alloys in Steam Environment at 1400 ℃(PDF)

MATERIALS CHINA[ISSN:1674-3962/CN:61-1473/TG]

Issue:
2026年11
Page:
1187-1195
Research Field:
Publishing date:

Info

Title:
Oxidation Failure Behavior of Cr-Coated Zirconium Alloys in Steam Environment at 1400 ℃
Author(s):
DENG Jianxi; HUO Shangle; SUN Qiaoyan; SONG Zhongxiao
State Key Laboratory for Mechanical Behavior of Materials, Xi’an Jiaotong University, Xi’an 710049, China
Keywords:
zirconium alloy claddings;  metal Cr coating;  high temperature steam oxidation;  coating failure;  eutectic reaction
CLC:

PACS:
TG146.4+14;TL352.2+2;TG174.4
DOI:
10.7502/j.issn.1674-3962.202607015
DocumentCode:

Abstract:
Cr coating with a thickness of approximately 13 μm was deposited on the surface of Zr-1Nb alloy cladding tubes via magnetron sputtering method. High-temperature oxidation tests of the Cr-coated zirconium alloy were performed for 5~30 min in 1400 ℃ steam environment using a thermogravimetric analyzer, with uncoated specimens set as the control group. Combined with characterization techniques including EBSD, SEM, EDS and EPMA, the evolution of the layered structure of the Cr coating, the diffusion behaviors of Cr, Zr and O elements, and the coating failure mechanism induced by the Cr-Zr eutectic reaction during oxidation were systematically investigated. The results demonstrate that as oxidation time extends from 5 to 30 min in 1400 ℃ steam environment, the layered structure of the Cr coating transforms from a threelayer mixed structure composed of Cr2O3/ZrO2, Cr/ZrO2 and Cr-Zr/ZrO2 into a three-layer oxide containing of ZrO2/Cr2O3, ZrO2 and Cr2O3. At ultra-high temperatures, the formation of Cr-Zr eutectic liquid phase induces void formation and coating delamination at the Cr coating/Zr substrate interface,resulting in the loss of protective properties of the coating as early as 5 min oxidation. The coupling effect of intense element diffusion, redox reaction and eutectic reaction at ultra-high temperatures causes high-rate linear oxidation kinetics of the Cr coated zirconium alloys.