[1]胡雅楠,张贤昆,翟明,等.铝/铜异种金属搅拌摩擦沉积增材制造异质界面微观组织与力学性能研究[J].中国材料进展,2026,45(12):001-9.
 HU Yanan,ZHANG Xiankun,ZHAI Ming,et al.Study on Heterogeneous Interfaces Microstructure and Mechanical Properties of Al/Cu Dissimilar Additive Friction Stir Deposition[J].MATERIALS CHINA,2026,45(12):001-9.
点击复制

铝/铜异种金属搅拌摩擦沉积增材制造异质界面微观组织与力学性能研究()

中国材料进展[ISSN:1674-3962/CN:61-1473/TG]

卷:
45
期数:
2026年12
页码:
001-9
栏目:
出版日期:
2026-11-30

文章信息/Info

Title:
Study on Heterogeneous Interfaces Microstructure and Mechanical Properties of Al/Cu Dissimilar Additive Friction Stir Deposition
作者:
胡雅楠; 张贤昆; 翟明; 武传松; 石磊
1.山东大学 材料液固结构演变与加工教育部重点实验室, 山东 济南 250061 2.中国铁道科学研究院集团有限公司金属及化学研究所,北京 100081
Author(s):
HU Yanan;  ZHANG Xiankun;  ZHAI Ming;  WU Chuansong;  SHI Lei
1. Key Laboratory for Liquid-Solid Structural Evolution and Processing of Materials of Ministry of Education, Shandong University, Jinan 250061, China 2. Metals and Chemistry Research Institute, China Academy of Railway Sciences Co., Ltd., Beijing 100081, China
关键词:
搅拌摩擦增材; 铝/铜界面; 金属间化合物; 剪切强度
Keywords:
additive friction stir deposition;  Al/Cu interface;  intermetallic compounds;  shear strength
分类号:
TG456.9;TG146.2
文献标志码:
A
摘要:
采用搅拌摩擦增材制造(AFSD)工艺在铜基体表面沉积铝合金,研究了转速与行进速度对沉积层宏观成形、Al/Cu 界面反应行为及界面力学性能的影响。结果表明,工艺参数显著影响材料塑化程度、界面热输入以及塑化材料的流动与回填行为。较低转速条件下,铜侧热输入和塑性变形不足,沉积层易出现表面粗糙、边缘失稳及界面裂纹等缺陷;而过高转速或过低行进速度会导致单位长度热输入过大,引起材料过度软化、横向流动增强以及沉积层边缘外溢。随着转速提高或行进速度降低,Al/Cu 界面反应层厚度由 0.18逐渐增加至 1.54 μm,说明界面元素互扩散和金属间化合物(IMCs)生长明显增强。界面剪切强度在不同工艺参数组合下存在较大差异,其中 800 r/min–50 mm/min 条件下获得最佳综合性能,界面剪切强度达到 95 MPa。该参数条件下形成了较薄且连续的界面反应层,能够在保证界面冶金结合的同时有效抑制界面脆化。研究表明,适中的转速与行进速度匹配更有利于实现热输入、材料塑化与界面反应之间的平衡,从而获得成形稳定且界面性能优异的 Al/Cu 异种金属复合结构。
Abstract:
Additive friction stir deposition (AFSD) was employed to deposit aluminum alloy onto a copper substrate, and the effects of rotational speed and travel speed on the macro-forming quality, interfacial reaction behavior, and mechanical properties of the Al/Cu interface were systematically investigated. The results indicated that the processing parameters significantly affected the material plasticization behavior, interfacial heat input, and the flow and refill behavior of the plasticized material. Under low rotational speed conditions, insufficient heat input and plastic deformation on the copper side resulted in surface roughness,edge instability, and interfacial cracking defects. In contrast, excessively high rotational speed or excessively low travel speed led to excessive heat input per unit length, causing severe materials softening, enhanced lateral material flow,and edge overflow of the deposited layer. With increasing rotational speed or decreasing travel speed, the thickness of the Al/Cu interfacial reaction layer increased from 0.18 to 1.54 μm gradually, indicating enhanced elemental interdiffusion and growth of intermetallic compounds (IMCs). The interfacial shear strength varied considerably among different combinations of process parameters, with the optimal overall performance being achieved at 800 r/min–50 mm/min where the interfacial shear strength reached 95 MPa. Under this condition, a thin and continuous interfacial reaction layer was formed, which effectively balanced metallurgical bonding and suppression of interfacial embrittlement. The results demonstrate that an appropriate combination of rotational speed and travel speed is beneficial for achieving a balance among heat input, material plasticization, and interfacial reaction behavior, thereby obtaining Al/Cu dissimilar structures with stable forming quality and superior interfacial properties.
更新日期/Last Update: 2026-10-30