[1]乔柯,陈帅军,王文,等.时效时间对搅拌摩擦沉积增材6061铝合金微观组织及力学性能的影响[J].中国材料进展,2026,45(12):040-49.
QIAO Ke,CHEN Shuaijun,WANG Wen,et al.Effect of Aging Time on Microstructure and Mechanical Properties of 6061 Aluminum Alloy Fabricated by Additive Friction Stir Deposition[J].MATERIALS CHINA,2026,45(12):040-49.
点击复制
时效时间对搅拌摩擦沉积增材6061铝合金微观组织及力学性能的影响()
中国材料进展[ISSN:1674-3962/CN:61-1473/TG]
- 卷:
-
45
- 期数:
-
2026年12
- 页码:
-
040-49
- 栏目:
-
- 出版日期:
-
2026-11-30
文章信息/Info
- Title:
-
Effect of Aging Time on Microstructure and Mechanical Properties of 6061 Aluminum Alloy Fabricated by Additive Friction Stir Deposition
- 作者:
-
乔柯; 陈帅军; 王文; 董继红; 等。
-
1.西安建筑科技大学冶金工程学院,陕西 西安 710055
2.功能材料加工国家地方联合工程研究中心,陕西 西安 710055
3.中国航空制造技术研究院,北京 100020
4.中车长春轨道客车股份有限公司,吉林 长春 130062
- Author(s):
-
QIAO Ke; CHEN Shuaijun; WANG Wen; DONG Jihong; et al.
-
1. College of Metallurgical Engineering,Xi’an University of Architecture and Technology, Xi’an 710055, China
2.National and Local Joint Engineering Research Center for Functional Materials Processing, Xi’an 710055, China
et al.
-
- 关键词:
-
6061铝合金; 搅拌摩擦沉积增材; 热处理; 微观组织; 力学性能
- Keywords:
-
6061 aluminum alloy; additive friction stir deposition; heat treatment; microstructure; mechanical properties
- 文献标志码:
-
A
- 摘要:
-
采用搅拌摩擦沉积增材制造(AFSD)技术制备了6061铝合金增材体,随后进行了“固溶+时效”处理,研究了时效时间对AFSD制备6061铝合金的微观组织及力学性能的影响。结果表明,AFSD过程中材料在摩擦热与剧烈塑性变形共同作用下发生连续动态再结晶,形成了细小等轴晶组织。增材体平均晶粒尺寸为2.43 μm,再结晶晶粒占比达到74.0%。6061铝合金增材体显微硬度为77 HV,抗拉强度和屈服强度分别为252和138 MPa。530 ℃固溶处理后经175 ℃时效12 h后,增材体晶粒尺寸增加至3.79 μm,同时形成了大量弥散分布的GP区以及Mg2Si纳米析出相,增材体显微硬度为124 HV,抗拉强度和屈服强度提升至326和254 MPa,主要归因于细晶强化与析出强化的协同作用。
- Abstract:
-
6061 aluminum alloy deposits were fabricated by additive friction stir deposition (AFSD) method and subsequently subjected to solution and aging treatments. The effect of aging time on the microstructural evolution and mechanical properties of AFSD-fabricated 6061 aluminum alloy was investigated. The results showed that continuous dynamic recrystallization occurred during the AFSD process under the combined effects of frictional heat and severe plastic deformation, resulting in a fine equiaxed grain structure. The average grain size of the deposit was 2.43 μm, and the fraction of recrystallized grains reached 74.0%. The deposit exhibited a microhardness of 77 HV, while the ultimate tensile strength and yield strength were 252 and 138 MPa, respectively. After aging at 175 °C for 12 h following solution at 530 ℃, the average grain size increased to 3.79 μm, accompanied by the formation of a large number of dispersed GP zones and nanoscale Mg2Si precipitates. The microhardness reached 124 HV, and the ultimate tensile strength and yield strength increased to 326 and 254 MPa, respectively. The improvement in mechanical properties was mainly attributed to the synergistic effect of grain refinement strengthening and precipitation strengthening.
更新日期/Last Update:
2026-11-02