[1]刘方媛,蒋磊,黄靖博,等.搅拌摩擦沉积增材 6061Al/TC4Ti异种合金界面组织与性能[J].中国材料进展,2026,45(12):010-19.
Liu Fangyuan,Jiang Lei,Huang Jingbo,et al.Interfacial Microstructure and Properties of 6061Al/TC4Ti Dissimilar Alloys Fabricated by Additive Friction Stir Deposition[J].MATERIALS CHINA,2026,45(12):010-19.
点击复制
搅拌摩擦沉积增材 6061Al/TC4Ti异种合金界面组织与性能()
中国材料进展[ISSN:1674-3962/CN:61-1473/TG]
- 卷:
-
45
- 期数:
-
2026年12
- 页码:
-
010-19
- 栏目:
-
- 出版日期:
-
2026-11-30
文章信息/Info
- Title:
-
Interfacial Microstructure and Properties of 6061Al/TC4Ti Dissimilar Alloys Fabricated by Additive Friction Stir Deposition
- 作者:
-
刘方媛; 蒋磊; 黄靖博; 吕万程等。
-
1.南京航空航天大学 材料科学与技术学院,江苏 南京 211106
2.再制造技术全国重点实验室,江苏 南京 211106
- Author(s):
-
Liu Fangyuan; Jiang Lei; Huang Jingbo; Lyu Wancheng; et al
-
1.College of Materials Science and Technology,Nanjing University of Aeronautics and Astronautics,Nanjing 211106,China
2.National Key Laboratory for Remanufacturing(NKLR),Nanjing 211106,China
-
- 关键词:
-
搅拌摩擦沉积增材; 6061铝合金; TC4钛合金; 界面组织; 金属间化合物; 力学性能
- Keywords:
-
Additive friction stir deposition; 6061 aluminum alloy; TC4 titanium alloy; Interfacial microstructure; Intermetallic compound; Mechanical properties.
- 文献标志码:
-
A
- 摘要:
-
6061铝合金与 TC4钛合金因密度、熔点及热膨胀系数差异显著,传统熔化焊易在界面生成脆性金属间化合物(如 TiAl3、TiAl、Ti3Al)而导致接头性能不足。本研究采用搅拌摩擦沉积增材(AFSD)技术制备了 6061Al/TC4Ti异种合金板材,重点考察了界面微观组织、元素分布及拉伸断裂行为。SEM-BSE观察显示,沿沉积方向各取样位置的 Al/Ti界面连续致密,局部呈波浪状起伏,未见宏观裂纹或孔洞。EDS线扫与面扫分析表明,Al与 Ti元素在约 2–3 μm范围内连续过渡,Si沿界面形成带状富集;EBSD结果显示,界面邻近区晶粒明显细化,尺寸主要集中于1–5 μm,Al侧和Ti侧大角度晶界(>15°)占比分别为50.9%和61.0%,表明AFSD强剪切与热循环促进了动态再结晶。拉伸试样抗拉强度为 158.5±3.5 MPa,延伸率为 14.6±2.9%,所有试样均在 Al侧断裂,断口以等轴深韧窝为主,呈韧性断裂特征,Al/Ti异质界面未成为优先失效位置。本工作在单一工艺参数下验证了 AFSD制备 Al/Ti固相复合板材的可行性,为后续系统优化工艺参数提供了基础数据。
- Abstract:
-
Due to the significant differences in density, melting point, and thermal expansion coefficient, traditional fusion welding of 6061 aluminum alloy and TC4 titanium alloy easily produces brittle intermetallic compounds at the interface (such as TiAl3, TiAl, Ti3Al), resulting in insufficient joint performance.In this study, 6061Al/TC4Ti dissimilar alloy composite plates were prepared using the additive friction stir deposition (AFSD) technique, with a focus on the interfacial microstructure, elemental distribution, and tensile fracture behavior. SEM-BSE observations showed that the Al/Ti interface at various sampling positions along the deposition direction was continuous and dense, with local undulating fluctuations, and no macroscopic cracks or pores were observed. EDS line scans and area scans indicated that Al and Ti elements transitioned continuously over a range of approximately 2–3 μm, with Si forming banded enrichment along the interface. EBSD results revealed significant grain refinement in the regions near the interface, with grain sizes mainly ranging from 1–5 μm. The proportions of large-angle grain boundaries (>15°) on the Al side and Ti side were 50.9% and 61.0%, respectively,indicating that the strong shear and thermal cycling of AFSD promoted dynamic recrystallization. The tensile specimens exhibited an ultimate tensile strength of 158.5 ± 3.5 MPa and an elongation of 14.6 ± 2.9%, with all specimens fracturing on the Al side. The fracture surfaces were dominated by equiaxed deep dimples, showing ductile fracture characteristics, and the Al/Ti heterogeneous interface did not act as a preferential failure location. This work verified the feasibility of preparing Al/Ti solid-state composite plates using AFSD under a single set of process parameters and provided foundational data for subsequent systematic optimization of process parameters