[1]沈祥福,马良超,刘桂涛,等.T6热处理对7075铝合金FSAM构件组织与性能的影响[J].中国材料进展,2026,45(12):020-29.
SHEN Xiangfu,MA Liangchao,LIU Guitao,et al.Effect of T6 Heat Treatment on the Microstructure and Properties of 7075 Aluminum Alloy FSAM Components[J].MATERIALS CHINA,2026,45(12):020-29.
点击复制
T6热处理对7075铝合金FSAM构件组织与性能的影响()
中国材料进展[ISSN:1674-3962/CN:61-1473/TG]
- 卷:
-
45
- 期数:
-
2026年12
- 页码:
-
020-29
- 栏目:
-
- 出版日期:
-
2026-11-30
文章信息/Info
- Title:
-
Effect of T6 Heat Treatment on the Microstructure and Properties of 7075 Aluminum Alloy FSAM Components
- 作者:
-
沈祥福; 马良超; 刘桂涛; 程英晔; 等。
-
1. 中国兵器科学研究院宁波分院,浙江 宁波 3151033
2. 西北工业大学 材料学院,陕西 西安 710000
- Author(s):
-
SHEN Xiangfu; MA Liangchao; LIU Guitao; CHENG Yingye; et al.
-
1. Ningbo Branch of Chinese Academy of Ordnance Science, Ningbo 315000, China
2. Northwest Institute for Nonferrous Metal Research, Xi’an 710000, China
-
- 关键词:
-
:7075铝合金; 搅拌摩擦增材制造; T6热处理; 析出强化; 强化机制
- Keywords:
-
7075 aluminum alloy; friction stir additive manufacturing; T6 heat treatment; precipitation strengthening; strengthening mechanism
- 文献标志码:
-
A
- 摘要:
-
采用送棒式搅拌摩擦增材(FSAM)技术制备7075铝合金构件,并对其进行T6热处理,研究了增材及T6热处理后构件的组织演化规律、力学性能变化及强化机制。结果表明:FSAM构件轴肩作用区域内未发现明显孔洞及层间分离现象,具有良好的成形质量。增材构件由细小等轴再结晶晶粒组成,顶部、中部和底部平均晶粒尺寸分别为2.53、2.82和3.84μm,受累积热循环影响,底部区域出现一定程度晶粒粗化。经T6热处理后,构件晶粒尺寸增大至4.07、4.05和4.73μm,组织均匀性提高。增材构件横截面的显微硬度为106~161HV,平均硬度122HV;经T6热处理后,构件显微硬度提高至174~186HV,平均硬度达到178HV。LD方向抗拉强度由419MPa提高至547MPa,BD方向由390MPa提高至497MPa,但塑性明显下降。TEM结果表明,FSAM过程中原有η′强化相发生回溶,组织中主要保留Al-Cr-Cu富集相;经T6热处理后,基体内重新析出大量弥散分布的η′强化相,同时保留热稳定的Cr富析出相,形成多尺度析出相。强化机制分析表明,FSAM构件强度主要来源于晶粒细化强化和位错强化;T6热处理后,析出强化贡献超过200MPa,成为强度提升的主导因素。断口分析及EBSD结果表明,粗大析出相引起的应力集中以及热处理后晶界微裂纹的存在是塑性下降的重要原因。
- Abstract:
-
7075 aluminum alloy components were fabricated using the rod-fed friction stir additive manufacturing (FSAM) technique and subsequently subjected to T6 heat treatment. The microstructural evolution, changes in mechanical properties, and strengthening mechanisms of the as-fabricated and T6-treated components were investigated. The results show that no obvious pores or interlayer separation were observed within the shoulder-affected region of the FSAM component, indicating good forming quality. The as-fabricated component consisted of fine equiaxed recrystallized grains, with average grain sizes of 2.53, 2.82, and 3.84μm at the top, middle, and bottom regions, respectively. A certain degree of grain coarsening occurred in the bottom region owing to the effect of accumulated thermal cycles. After T6 heat treatment, the grain sizes increased to 4.07, 4.05, and 4.73μm, accompanied by improved microstructural uniformity. The microhardness of the as-fabricated component ranged from 106 to 161HV, with an average value of 122HV, while that after T6 heat treatment increased to 174~186HV, reaching an average of 178HV. The ultimate tensile strength in the LD direction increased from 419MPa to 547MPa, while that in the BD direction increased from 390MPa to 497MPa, accompanied by a significant reduction in ductility. TEM results revealed that the original η′ strengthening precipitates underwent dissolution during FSAM, leaving mainly Al-Cr-Cu-rich phases in the microstructure. After T6 heat treatment, a large number of finely dispersed η′ strengthening precipitates re-precipitated in the matrix, while thermally stable Cr-rich precipitates were retained, resulting in a multiscale precipitate structure. Analysis of the strengthening mechanisms indicated that the strength of the as-fabricated component was mainly derived from grain refinement strengthening and dislocation strengthening. After T6 heat treatment, precipitation strengthening contributed more than 200MPa and became the dominant factor responsible for the increase in strength. Fracture analysis and EBSD results indicated that stress concentration caused by coarse precipitates and the presence of microcracks at grain boundaries after heat treatment were important factors contributing to the reduction in ductility.
更新日期/Last Update:
2026-11-02