[1]孙立成,刘恢弘,胡亦冉,等.高强塑纯Zn构件的搅拌摩擦沉积制造[J].中国材料进展,2026,45(12):050-59.
SUN Licheng,LIU Huihong,HU Yiran,et al.Friction Stir Deposition of Strong and Ductile Pure Zn Components[J].MATERIALS CHINA,2026,45(12):050-59.
点击复制
高强塑纯Zn构件的搅拌摩擦沉积制造()
中国材料进展[ISSN:1674-3962/CN:61-1473/TG]
- 卷:
-
45
- 期数:
-
2026年12
- 页码:
-
050-59
- 栏目:
-
- 出版日期:
-
2026-11-30
文章信息/Info
- Title:
-
Friction Stir Deposition of Strong and Ductile Pure Zn Components
- 作者:
-
孙立成; 刘恢弘; 胡亦冉; 张彦; 等。
-
1上海交通大学,上海市复杂薄板结构数字化制造重点实验室,上海,200240
2上海市第六人民医院,上海交通大学医学院附属第六人民医院,上海,200233
- Author(s):
-
SUN Licheng; LIU Huihong; HU Yiran; ZHANG Yan; et al.
-
1 Shanghai Key Laboratory of Digital Manufacture for Thin-walled Structures, Shanghai Jiao Tong University, Shanghai, 200240, China
2 Shanghai Sixth People’s Hospital Affiliated to Shanghai Jiao Tong University School of Medicine, Shanghai 200233, China
-
- 关键词:
-
可降解Zn构件; 螺杆挤出塑化搅拌摩擦沉积; 过程信号; 微观组织; 力学性能
- Keywords:
-
biodegradable pure Zn components; screw extrusion-plasticizing friction stir deposition; process signals; microstructure; mechanical properties
- 文献标志码:
-
A
- 摘要:
-
Zn及其合金被认为是极具发展前景的新一代可降解医用金属材料。熔化增材制造虽可实现复杂形状定制,但易受凝固缺陷影响,力学性能受限;大塑性变形固相加工可优化组织性能,但构件尺寸形状受限。本文采用螺杆挤出塑化搅拌摩擦沉积(SEFSD)工艺,以纯Zn颗粒为原料制备沉积墙,研究沉积过程物理信号、组织演化及构件力学性能。结果表明,沉积过程中沉积层金属的旋转搅动与顶锻铺展使扭矩和轴向力升高;沉积墙以动态再结晶微米级等轴细晶为主,并保留较高位错密度;构件x方向抗拉强度为171.9±15.5 MPa,延伸率为27±4%。SEFSD兼具固相组织调控和增材制造近净成形优势,为可降解Zn构件的高性能制造提供了新思路。
- Abstract:
-
Zn and its alloys are considered promising next-generation biodegradable metals for biomedical applications. Although fusion-based additive manufacturing enables the customization of complex geometries, solidification defects often limit the resulting mechanical properties. Solid-state processing through severe plastic deformation can improve microstructures and properties, but the attainable sizes and geometries of components remain limited. Here, a deposition wall was fabricated from pure Zn particles using screw extrusion-plasticizing friction stir deposition (SEFSD). We investigated the process signals, microstructural evolution, and mechanical properties of the deposited component. During deposition, the rotational stirring and forging-assisted spreading of the deposited metal increased both the torque and axial force. The deposition wall consisted predominantly of dynamically recrystallized, micron-scale equiaxed grains and retained a relatively high dislocation density. Along the x direction, the component exhibited a tensile strength of 171.9 ± 15.5 MPa and an elongation of 27 ± 4%. By combining solid-state microstructural control with the near-net-shape capability of additive manufacturing, SEFSD provides a new route for the high-performance manufacturing of biodegradable Zn components.
更新日期/Last Update:
2026-11-02