[1]李玉莉,陈晓峰,韩雪,等.微纳米生物玻璃的体外成骨性能研究[J].中国材料进展,2012,(6):007-11.[doi:10.7502/j.issn.1674-3962.2012.06.02]
 LI Yuli,CHEN Xiaofeng,HAN Xue,et al. Biocompatibility and Osteogenesis of Micro and Nano Bioactive Glasses[J].MATERIALS CHINA,2012,(6):007-11.[doi:10.7502/j.issn.1674-3962.2012.06.02]
点击复制

微纳米生物玻璃的体外成骨性能研究()
分享到:

中国材料进展[ISSN:1674-3962/CN:61-1473/TG]

卷:
期数:
2012年第6期
页码:
007-11
栏目:
前沿综述
出版日期:
2012-06-25

文章信息/Info

Title:
 Biocompatibility and Osteogenesis of Micro and Nano Bioactive Glasses
作者:
李玉莉陈晓峰韩雪苗国厚胡庆雷波
(1.华南理工大学材料科学与工程学院, 广东 广州 510640)
(2.国家人体组织功能重建工程技术研究中心, 广东 广州 510006)
(3.广东省生物医学工程重点实验室, 广东 广州 510006)
Author(s):
LI Yuli123 CHEN Xiaofeng123 HAN Xue123 MIAO Guohou123 HU Qing123 LEI Bo123
(1.School of Materials Science and Engineering, South China University of Technology, Guangzhou 510641, China)
(2.National Engineering Research Center for Tissue Restoration and Reconstruction, Guangzhou 510006, China)
(3.Guangdong Province Key Laboratory of Biomedical Engineering, South China University of Technology, Guangzhou 510006, China)
关键词:
微纳米生物玻璃溶胶-凝胶技术碱性磷酸酶成骨基因
DOI:
10.7502/j.issn.1674-3962.2012.06.02
文献标志码:
A
摘要:
微纳米生物活性玻璃因其具有特殊的形态结构和理化性能目前引起众多研究者的关注,但是目前对微纳米生物活性玻璃的结构及形态对细胞性能的影响研究的较少。本文通过溶胶-凝胶法结合模板仿生技术合成了具有特殊结构和形态的微纳米生物活性玻璃,并通过体外细胞实验,研究了这种微纳米结构对人骨髓间充质干细胞成骨性能(ALP, Runx2, Col1a1 和OPN)的影响,结果证明具有规则形态的生物活性玻璃(SBG)相比不规则形态的生物活性玻璃(IBG)更能促进细胞的体外成骨性能,为将来设计具有特定结构的生物活性玻璃提供了参考依据。
Abstract:
Because of the special morphology and characterization, micro and nano bioactive glass caused much attention by researchers, but the morphology of micro and nano bioactive glass on cell performance has been underappreciated and underinvestigated. The special morphology of micro and nano bioactive glass was synthesized by the Sol gel method combined with the template bionic. Human mesenchymal stem cells (hMSCs) were seeded on bioactive glass for 6 days and 10 days in vitro for alkalic phosphatase (ALP) activity and 5days for osteogenic gene expression analysis. Based on the results of ALP activity and osteogenic gene expression analysis, the responses of hMSCs to the SBG exhibited a higher degree of osteogenic differentiation than those on IBG  in vitro. This work will provide a reference for design of specific morphology of the bioactive glass in the future.
更新日期/Last Update: 2012-07-26